Water basis - halogen free – ph 5.5 manufacture of batteries in the C.O.S. process

FLUXAK 1043 - Water basis - halogen free – ph 5.5 manufacture of batteries in the C.O.S. process

Non-Corrosive flux, intended for battery manufacturing in COS process, totally eliminated when dipped into the lead bath. The flux is formulated from pure organic compounds (in water solution). It is eliminated by sublimation in the range of temperatures where lead and alloys used for batteries manufacturing melt. Since no residual salts or combustion residues remain after soldering (casting), problems linked to conductivity (self-discharge) and corrosion are solved when using this technology.

  • Acuoso viscoso
  • Aleaciones de plomo
  • Lead alloys
  • Aleaciones de plomo
  • No
  • 280-480° C
  • Fundente orgánico sin halógeno, recomendado para soldadura de placas de plomo-calcio

CHARACTERISTICS - PHYSICO-CHEMICAL PROPERTIES, COMPOUND ELEMENTS

Liquid neutral flux halogen free, fully burnt off after heating and without residues COMPOSITION Secondary organic amine salts PHYSICO-CHEMICAL PROPERTIES Density at 20° C ≈1,11 g/cm3 pH = 5

PRODUCT APPLICATION

This flux is of particular interest for the manufacture of starter battery lead calcium and storage batteries where self-discharge phenomena must be avoided. It is a neutral flux and as such a multi purpose product intended to be used regardless of the type of strap and grid alloys.

DIRECTIONS FOR USE

The flux must be used undiluted on the surface of the lugs by dipping or impregnation.

USING CARE AND RECOMMENDATIONS

Without particular risk - Refer to health and safety datasheets before