Because of its specific formulation FLUXAK 1032 has a low acidity and a weak capillarity. Applied by impregnation, the electro-chemical effects are minimised and the risk of self discharge is prohibited.

  • Aqueous
  • Lead alloys
  • Lead alloys
  • Lead alloys
  • No
  • 350-500° C
  • Flux with low pickling power, low capillarity, for small batteries

CHARACTERISTICS - PHYSICO-CHEMICAL PROPERTIES, COMPOUND ELEMENTS

COMPOUNDS
Organic salts basis
PHYSICAL PROPERTIES

From colourless to pale yellow liquid

Density at 20°C : 1.200+/- 0.010
pH : 1

PRODUCT APPLICATIONS

This product is preferred to Fluxak 1029 when soldering conditions allow work at a very low acidity. The diffusion of the flux by capillarity is regulated by its low wettability on the pieces.

DIRECTIONS FOR USE

Fluxak 1032 is always used undiluted, The quantity of flux deposited on the lugs is minimal. Whatever fluxing process is used (dipping bath or impregnated sponge) the level of flux impregnation should not be more than 1-2mm maximum. Therefore, the machines should be set up in such a way that they only depose a very small quantity of flux on the lugs.

USING CARE AND RECOMMENDATIONS